Cast copper alloy C93700 (Bearing Bronze)
Chemical composition: Sn=10.0%, Pb=9.5%, Cu=80%
Property Value in metric unit Value in US unit
Density 8.86 *10³ kg/m³ 553 lb/ft³
Modulus of elasticity 75.8 GPa 11000 ksi
Thermal expansion (20 ºC) 18.5*10-6 ºCˉ¹ 10.3*10-6 in/(in* ºF)
Specific heat capacity 377 J/(kg*K) 0.090 BTU/(lb*ºF)
Thermal conductivity 46.9 W/(m*K) 325 BTU*in/(hr*ft²*ºF)
Electric resistivity 17.0*10-8 Ohm*m 17.0*10-6 Ohm*cm
Tensile strength (sand cast) 290 MPa 42000 psi
Yield strength (sand cast) 145 MPa 21000 psi
Elongation (sand cast) 20 % 20 %
Hardness (sand cast) 77 HB(500) 77 HB(500)
Liquidus temperature 929 ºC 1705 ºF
Solidus temperature 762 ºC 1403 ºF