Cast copper alloy C86700 (Manganese Bronze)
Chemical composition: Zn=39%, Mn=1.8%, Fe=2.0%, Al=2.0%, Pb=1.0%, Cu=58%
Property Value in metric unit Value in US unit
Density 8.33 *10³ kg/m³ 520 lb/ft³
Modulus of elasticity 103 GPa 15000 ksi
Thermal expansion (20 ºC) 19.8*10-6 ºCˉ¹ 11.0*10-6 in/(in* ºF)
Specific heat capacity 377 J/(kg*K) 0.090 BTU/(lb*ºF)
Electric resistivity 10.3*10-8 Ohm*m 10.3*10-6 Ohm*cm
Tensile strength (sand cast) 586 MPa 85000 psi
Yield strength (sand cast) 290 MPa 42000 psi
Elongation (sand cast) 20 % 20 %
Hardness (sand cast) 155 HB(3000) 155 HB(3000)
Liquidus temperature 880 ºC 1616 ºF
Solidus temperature 862 ºC 1583 ºF