Synthetic Ester based hydraulic oil
Property Value in metric unit Value in US unit
Density at 60°F (15.6°C) 0.921 *10³ kg/m³ 57.5 lb/ft³
Kinematic viscosity at 104°F (40°C) 48.7 cSt 48.7 cSt
Kinematic viscosity at 212°F (100°C) 8.7 cSt 8.7 cSt
Viscosity index 160 160
Flash point 220 ºC 428 ºF
Pour Point -58 ºC -72 ºF
Zinc max.5 ppm max.5 ppm