Chlorinated solvent 1,1,1-trichloroethane (methyl chloroform)
Chemical formula: CH3-CCl
Property Value in metric unit Value in US unit
Density at 68°F (20°C) 1.34*10³ kg/m³ 83.6 lb/ft³
Viscosity at 68°F (20°C)) 0.87 cP 5.84*10-4 lb/ft·s
Surface tension at 77°F (25°C) 0.025 N/m 1.43*10-4 lbf/in
Vapor pressure at 68°F (20°C) 13300 Pa 1.93 psi
Boiling point 74 ºC 165 ºF
Melting Point -30 ºC -22 ºF
Autoignition temperature 537 ºC 999 ºF
Dielectric constant at 68°F (20°C) 7.53 7.53
Specific heat capacity 926 J/(kg*K) 0.221 BTU/(lb*ºF)
Latent heat of vaporization 243 kJ/kg 104.5 BTU/lb