to Hydrocarbon solvents
to Properties of fluids
(submitted by the website administration)
| Aromatic solvent Xylene | ||||
| Chemical formula: C8H10 | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density at 68°F (20°C) | 0.88 *10³ | kg/m³ | 54.9 | lb/ft³ |
|---|---|---|---|---|
| Viscosity at 68°F (20°C) | 0.81 | cP | 5.44*10-4 | lb/ft·s |
| Surface tension at 68°F (20°C) | 0.030 | N/m | 1.71*10-4 | lbf/in |
| Vapor pressure at 68°F (20°C) | 6 | torr | 6 | torr |
| Boiling point | 144.4 | ºC | 291.9 | ºF |
| Melting Point | -25 | ºC | -13 | ºF |
| Flash Point | 32 | ºC | 90 | ºF |
| Dielectric constant at 77°F (25°C) | 2.57 | 2.57 | ||
| Dipole moment at 68°F (20°C) | 0.45 | Debye | 0.45 | Debye |
| Color | Colorless | Colorless | ||