Wrought aluminum-lithium alloy Weldalite 049 | ||||
Chemical composition: Li=1.3%, Cu=4.5%, Mg=0.4% Zr=0.14%, Ag=0.4%, Al balance | ||||
Property | Value in metric unit | Value in US unit | ||
Density | 2.6 *10³ | kg/m³ | 162 | lb/ft³ |
---|---|---|---|---|
Tensile strength | 480 | MPa | 69600 | psi |
Yield strength | 330 | MPa | 47900 | psi |
Elongation | 24 | % | 24 | % |
Shear strength | 290 | MPa | 42100 | psi |
Hardness | 129 | HB | 129 | HB |
Tensile strength (T6) | 720 | MPa | 104000 | psi |
Yield strength (T6) | 680 | MPa | 98600 | psi |
Elongation (T6) | 4 | % | 4 | % |
Shear strength (T6) | 420 | MPa | 60900 | psi |
Fracture toughness (T6) | 30 | MPa*m½ | 27.3 | ksi*in½ |