Chemical formula: CH3I
Property Value in metric unit Value in US unit
Density at 68°F (20°C) 2.27*10³ kg/m³ 142 lb/ft³
Vapor pressure at 68°F (20°C) 50 kPa 7.3 psi
Boiling point 42 ºC 108 ºF
Melting Point -66 ºC -88 ºF