to Metal Matrix Composites (introduction)
to Properties of composites
| Metal Matrix Composite Al-60% Al2O3 fiber | ||||
| Composition: Pure aluminum+ 60 vol.% Al2O3 continuous fibers | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 3.4 *10³ | kg/m³ | 212 | lb/ft³ |
|---|---|---|---|---|
| Modulus of elasticity (long.) | 240 | GPa | 34800 | ksi |
| Modulus of elasticity (trans.) | 130 | GPa | 18850 | ksi |
| Tensile strength (longitude.) | 1600 | MPa | 232050 | psi |
| Compressive strength (long.) | 1700 | MPa | 246600 | psi |