High thermal conductivity isostatically pressed graphite

(submitted by the website administration)

High thermal conductivity isostatically pressed graphite
Chemical composition: carbon (C)
Property Value in metric unit Value in US unit
Density 1.90*10³ kg/m³ 119 lb/ft³
Modulus of elasticity 11.8 GPa 1710 ksi
Flexural strength 53.9 MPa 7820 psi
Compressive strength 103 MPa 14940 psi
Tensile strength 29.4 MPa 4260 psi
Hardness (Shore) 60 HS 60 HS
Thermal expansion (20 ºC) 4.8*10-6 ºCˉ¹ 2.7*10-6 in/(in* ºF)
Thermal conductivity 139 W/(m*K) 963 BTU*in/(hr*ft²*ºF)
Electric resistivity 9.5*10-6 Ohm*m 9.5*10-4 Ohm*cm


Applications: Non-ferrous metals metallurgy and semiconductors fabrication.