Extractive metallurgy of nickel

Dr. Dmitri Kopeliovich

Nickel occurs in ores of two general types:

Both of them typically contain 1-3% of nickel.

Extraction of nickel from sulfide ores

Extraction of nickel from sulfide oresis carried out by the following process:

This operation is conducted in a flotation chamber where the ground ore mixed with water is treated by air bubbles which move upward and cause flotation of the mineral particles to the top of the chamber.

At this stage the concentrate is smelted in the Bessemer converter to produce a mixture of nickel, copper and other metals called matte.

The gangue is absorbed by the slag and removed.

Extraction of nickel from the laterite ores

Extraction of nickel from the laterite ores is carried out by either pyrometallurgical or hydrometallurgical process: