| Coarse grade extruded graphite | ||||
| Chemical composition: carbon (C) | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 1.55*10³ | kg/m³ | 96.8 | lb/ft³ |
|---|---|---|---|---|
| Grain size | 6.35 | mm | 0.25 | inch |
| Flexural strength | 8.3 | MPa | 1200 | psi |
| Electric resistivity | 7.6*10-6 | Ohm*m | 7.6*10-4 | Ohm*cm |
Applications: kiln lubrication block, welding plates, side-wall liner, extrusion plates.