| Alumina aerogel monolith | ||||
| Chemical composition: Al2O3, derived from aluminum alkoxide, %Solids: 2% | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 0.037 *10³ | kg/m³ | 2.3 | lb/ft³ |
|---|---|---|---|---|
| Internal Surface Area | 376 | m²/g | 1.8*106 | ft²/lb |
| Modulus of elasticity | 0.00055 | GPa | 0.08 | ksi |
| Thermal conductivity (100ºF/38ºC) | 0.029 | W/(m*K) | 0.20 | BTU*in/(hr*ft²*ºF) |