Aromatic solvent Xylene
Chemical formula: C8H10
Property Value in metric unit Value in US unit
Density at 68°F (20°C) 0.88 *10³ kg/m³ 54.9 lb/ft³
Viscosity at 68°F (20°C) 0.81 cP 5.44*10-4 lb/ft·s
Surface tension at 68°F (20°C) 0.030 N/m 1.71*10-4 lbf/in
Vapor pressure at 68°F (20°C) 6 torr 6 torr
Boiling point 144.4 ºC 291.9 ºF
Melting Point -25 ºC -13 ºF
Flash Point 32 ºC 90 ºF
Dielectric constant at 77°F (25°C) 2.57 2.57
Dipole moment at 68°F (20°C) 0.45 Debye 0.45 Debye
Color Colorless Colorless