Wrought aluminum-zinc-magnesium alloy 7072 | ||||
Chemical composition: Zn=1.0%, Al balance | ||||
Property | Value in metric unit | Value in US unit | ||
Density | 2.72 *10³ | kg/m³ | 170 | lb/ft³ |
---|---|---|---|---|
Modulus of elasticity | 70 | GPa | 10200 | ksi |
Thermal expansion (20 ºC) | 23.6*10-6 | ºCˉ¹ | 13.1*10-6 | in/(in* ºF) |
Specific heat capacity | 893 | J/(kg*K) | 0.213 | BTU/(lb*ºF) |
Thermal conductivity | 222 | W/(m*K) | 1540 | BTU*in/(hr*ft²*ºF) |
Electric resistivity | 2.99*10-8 | Ohm*m | 2.99*10-6 | Ohm*cm |
Tensile strength (annealed) | 70 | MPa | 10200 | psi |
Elongation (annealed) | 15 | % | 15 | % |
Shear strength (annealed) | 55 | MPa | 8000 | psi |
Hardness (annealed) | 20 | HB | 20 | HB |
Tensile strength (H12) | 100 | MPa | 14500 | psi |
Yield strength (H12) | 68 | MPa | 9860 | psi |
Shear strength (H12) | 60 | MPa | 8700 | psi |
Hardness (H12) | 28 | HB | 28 | HB |
Annealing temperature | 343 | ºC | 650 | ºF |