Spinodal Bronze Nicomet
Chemical composition: Ni=5.75%, Sn=5.75%, Zn=1.75%, Cu=balance
Property Value in metric unit Value in US unit
Density 8.86 *10³ kg/m³ 553 lb/ft³
Thermal conductivity 53.7 W/(m*K) 372 BTU*in/(hr*ft²*ºF)
Electric conductivity 12% I.A.C.S. 12% I.A.C.S.
Tensile strength 517 MPa 75000 psi
Yield strength 345 MPa 50000 psi
Elongation 5 % 5 %
Hardness 90 RB 90 RB