Composition: Pure aluminum+ 60 vol.% Al2O3 continuous fibers
Property Value in metric unit Value in US unit
Density 3.4 *10³ kg/m³ 212 lb/ft³
Modulus of elasticity (long.) 240 GPa 34800 ksi
Modulus of elasticity (trans.) 130 GPa 18850 ksi
Tensile strength (longitude.) 1600 MPa 232050 psi
Compressive strength (long.) 1700 MPa 246600 psi