Low temperature hydraulic oil ISO 22

(submitted by the website administration)

Low temperature hydraulic oil ISO 22
Mineral based hydraulic oil
Property Value in metric unit Value in US unit
Density at 60°F (15.6°C) 0.864 *10³ kg/m³ 53.9 lb/ft³
Kinematic viscosity at 104°F (40°C) 21.6 cSt 21.6 cSt
Kinematic viscosity at 212°F (100°C) 4.23 cSt 4.23 cSt
Viscosity index 99 99
Flash point 208 ºC 406 ºF
Pour Point -36 ºC -33 ºF
Aniline Point 98 ºC 208 ºF
Color max. 1.5 max. 1.5