Low porosity isostatically pressed graphite

(submitted by the website administration)

Low porosity isostatically pressed graphite
Chemical composition: carbon (C)
Property Value in metric unit Value in US unit
Density 1.87*10³ kg/m³ 117 lb/ft³
Porosity 6 % 6 %
Modulus of elasticity 12.5 GPa 1810 ksi
Flexural strength 50 MPa 7250 psi
Compressive strength 105 MPa 1522 0 psi
Hardness (Shore) 65 HS 65 HS
Thermal expansion (20 ºC) 4.2*10-6 ºCˉ¹ 2.3*10-6 in/(in* ºF)
Thermal conductivity 110 W/(m*K) 762 BTU*in/(hr*ft²*ºF)
Electric resistivity 12*10-6 Ohm*m 12*10-4 Ohm*cm


Applications: Continuous casting molds for copper alloys (Cu, CuSn, CuZn), silver, gold.