Mineral based gear oil
Property Value in metric unit Value in US unit
Density at 60°F (15.6°C) 0.884 *10³ kg/m³ 55.2 lb/ft³
Kinematic viscosity at 104°F (40°C) 149.7 cSt 149.7 cSt
Kinematic viscosity at 212°F (100°C) 14.8 cSt 14.8 cSt
Viscosity index 98 98
Timken OK load 27.5 kg 60.6 lb.
Flash point 256 ºC 493 ºF
Pour Point -24 ºC -11 ºF
AGMA No. 4EP 4EP
Color 3.5 3.5