Fabrication of Metal Matrix Composites by co-deposition

Dr. Dmitri Kopeliovich

Co-deposition is a process, in which matrix metal is deposited together with the dispersed phase by one of the deposition techniques.

The following co-deposition methods are used for manufacturing Metal Matrix Composites:

Electrolytic co-deposition

This method (Electrolytic co-deposition) involves Electroplating technique, in which electrolyte solution of matrix metal ions contains suspended particles of dispersed phase. When the matrix metal is deposited on a substrate, the dispersed phase particles are entrapped by the coating, reinforcing the matrix material.

Examples of electrolytic co-deposition:

  • Ni-Al2O3 - oxidation resistant nickel matrix composite;
  • Ni-SiC – wear resistant nickel matrix composite;
  • Ni-PTFE, Ni-C, Ni-MoS2 – antifriction nickel matrix composites.
  • Anti-friction coating of Engine bearings consisting of lead-tin-copper alloy and reinforced by alumina (Al2O3) is fabricated by electrolytic co-deposition from electrolyte solution of lead, tin and copper with alumina particles.
  • Aluminum matrix material reinforced by silica (SiO2) is prepared from AlCl3-dimethylsulfone electrolyte containing fine silica particles.

to top

Spray co-deposition

This method implements Thermal spraying technique for atomizing molten matrix metal, droplets of which are delivered to a substrate in a high velocity gas stream together with dispersed phase particles supplied to the stream from a separate container.

The method allows fabrication of near-net-shape forming of Metal Matrix Composites.

Examples of spray co-deposition:

Aluminum matrix material reinforced by silicon carbide (SiC) is produced by spray co-deposition followed by Rolling.

High Velocity Oxyfuel Spraying (HVOS) method is used for fabrication tungsten carbide-cobalt (WC-Co) composite material, which is conventionally manufactured by more expensive technology of sintering fabrication of Metal Matrix Composites.

to top

Vapor co-deposition

Vapor co-deposition is a group of various methods, utilizing materials in vapor state: Physical Vapor Deposition (PVD), Chemical Vapor Deposition (CVD), Direct Vapor Deposition (DVD).

In these methods coating of solid material is formed as a result of vapor condensation or chemical reaction on a substrate surface.

Vapor co-deposition is used for coating fibers, creating multilayer depositions, fabricating nanostructure composite materials.

to top


Related internal links

fabrication_of_metal_matrix_composites_by_co-deposition.txt · Last modified: 2023/12/13 by dmitri_kopeliovich
Promote in SubsTech       Creative Commons License Except where otherwise noted, this work is licensed under a Creative Commons Attribution-Noncommercial-Share Alike 3.0 License