Extruded carbon

(submitted by the website administration)

Extruded carbon
Chemical composition: petroleum coke based baked carbon (C), ash 0.2%
Property Value in metric unit Value in US unit
Density 1.62*10³ kg/m³ 101 lb/ft³
Maximum grain size 760 μm 30 microinch
Flexural strength 15.9 MPa 2300 psi
Tensile strength 11.7 MPa 1700 psi
Compressive strength 38.5 MPa 5585 psi
Thermal conductivity 10 W/(m*K) 69.3 BTU*in/(hr*ft²*ºF)
Electric resistivity WG (with grain) 42*10-6 Ohm*m 42*10-4 Ohm*cm
Electric resistivity AG (against grain) 50*10-6 Ohm*m 50*10-4 Ohm*cm


Applications: anodes for electroplating, low thermal conductivity applications.

Related internal links

Related external links

extruded_carbon.txt · Last modified: 2012/09/01 by dmitri_kopeliovich
Promote in SubsTech       Creative Commons License Except where otherwise noted, this work is licensed under a Creative Commons Attribution-Noncommercial-Share Alike 3.0 License