Mineral oil and natural esters based fluid
Property Value in metric unit Value in US unit
Density at 60°F (15.6°C) 0.905 *10³ kg/m³ 56.5 lb/ft³
Kinematic viscosity at 104°F (40°C) 22.3 cSt 22.3 cSt
Flash point 182 ºC 360 ºF
Pour Point -20 ºC -4 ºF


Applications: machining of non-ferrous metals: aluminum, brass, bronze, copper, and magnesium.